0102030405
FAAV Keramyske A-klep
Wichtichste technyske parameters
| Ûnderdiel | Y-ZrO Y-TZP | Mg-ZrO₂ M-PSZ | 90 Al₂O₃ | 95 Al₂O₃ | 99 Al₂O₃ | Si₃N℄ | SiC | Gewoane keramyk | Karbidlegering | 45# Stiel |
| Dichtheid g/cm³ | 6.0~6.05 | 5.72~5.74 | 3.45~3.55 | 3.6~3.75 | 3.9~3.95 | 3.2~3.33 | 3.15~3.25 | 3.0~3.5 | 14~18 | 7.8 |
| Hurdens HRA/C | 87 | 85 | 90 | 90 | 92 | 92 | 94 | 50~60 | 70 | 36 |
| Bûgingssterkte MPa | 1150 | 900 | 350 | 370 | 450 | 1200 | 470 | 20~50 | 2000 | 804 |
| Breuktaaiens (KIC) MPa√m | 10~12 | 13~15 | 3.4 | 3.6 | 4.5 | 7 | 4 | -- | 20 | 101 |
| Kompresjesterkte MPa | 2000 | 1800 | 1700 | 2000 | 2200 | 2800 | -- | -- | 4000 | 2000 |
| Termyske skokbestindigens °C | 87 | 110 | -- | -- | 50 | 200 | 75 | -- | 500 | 500 |
| Termyske útwreidingskoëffisjint × 10⁻⁶/°C | 9.6 | 10 | 7.6 | 7.8 | 8.3 | 3.4 | 4 | -- | 7 | 12 |
| Elastisiteitsmodulus GPa | 200 | 200 | 310 | 330 | 350 | 300 | 400 | -- | 600 | -- |
| Ferpletterjende lading KN (Φ6mm) | 15 | 10 | 3.5 | 3.6 | 4 | 18 | 3.5 | -- | -- | -- |
| Temperatuer °C brûke | -- | -- | ||||||||
| Wetteropname | 0 | 0 | 0,02% | 0,01% | 0,00% | 0 | 0,50% | 5~10% | -- | -- |
| Korrosjeprevinsje | Goed | Goed | Goed | Goed | Goed | Goed | Goed | Flooey | Goed | Flooey |
*Gegevensboarnen: testresultaten of útjûne orizjinele dokuminten.

REFERINSJETABEL FOAR ANTI-KORROSIEF PRESTAASJES
| Media | Temperatuer | ZrO₂ | 99,9% Al₂O₃ | SiC | Si₃N℄ | Grafyt | PTFE | Fluorrubber | SS304 | SS316 | HC |
| 20% HCL | 60°C | IN | IN | IN | B | IN | IN | IN | C | C | B |
| 20% HCL | 95°C | IN | IN | IN | C | IN | IN | IN | -- | -- | C |
| 90% H₂SO₄ | 60°C | IN | IN | IN | IN | IN | IN | IN | C | C | B |
| 90% H₂SO₄ | 95°C | IN | IN | IN | B | IN | IN | IN | C | C | C |
| 60% H₃PO₄ | 60°C | IN | IN | IN | C | IN | IN | IN | C | C | IN |
| 60% H₃PO₄ | 95°C | IN | IN | IN | C | IN | IN | IN | C | C | IN |
| 10% HF | 60°C | C | B | IN | IN | IN | IN | IN | C | C | B |
| 46% HF | 95°C | C | C | IN | C | IN | IN | IN | -- | -- | C |
| 60% HNO₃ | 60°C | IN | IN | IN | C | B | IN | IN | IN | IN | C |
| 60% HNO₃ | 95°C | IN | B | IN | C | B | IN | IN | B | B | C |
| 30% NaOH | 60°C | IN | B | IN | B | IN | IN | IN | IN | IN | IN |
| 30% NaOH | 95°C | B | B | IN | C | IN | IN | IN | IN | B | IN |
In ≤ 0.1mmg/cm²/dei: Kin negearre wurde of hat gjin korrosje, oanrikkemandearre foar gebrûk.
B = 0.1~0.3mmg/cm²/dei: Lichte of tige lytse korrosje, brûk mei foarsichtigens.
C ≥ 0,3 mmg/cm²/dei: Signifikante korrosje, net oanrikkemandearre foar gebrûk.
-- : Yntinsive korrosje, foar safier't mjitting net mooglik is.
Flowkarakteristykblêd fan keramyske balklep
| Kearnspesifikaasjes | O-type balkearn | V60° balkearn | V45° balkearn | V30° balkearn |
| DN15 | 10 | 7 | 4 | 3 |
| DN20 | 18.2 | 12 | 8 | 5 |
| DN25 | 29 | 18 | 12 | 8 |
| DN32 | 47 | 30 | 20 | 13 |
| DN40 | 73 | 46 | 31 | 21 |
| DN50 | 114 | 72 | 48 | 32 |
| DN65 | 181 | 115 | 76 | 51 |
| DN80 | 292 | 185 | 123 | 82 |
| DN100 | 456 | 289 | 192 | 128 |
| DN125 | 712 | 452 | 300 | 201 |
| DN150 | 1025 | 650 | 432 | 289 |
| DN200 | 1822 | 1156 | 769 | 514 |